Description

Silicon carbide, mainly consisting of SiC, it maintains strength up to 1400°C and it is ideal for use as a construction material. SiC has excellent thermal conductivity, low thermal expansion and is very resistant to acids and lyes. It masters corrosion, abrasion and erosion as skillfully as it stands up to frictional wear.

This material data has been provided by Innovacera.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.02 g/cm³

Show Supplier Material materials with Density of 3.02 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

250 MPa

Show Supplier Material materials with Compressive strength of 250 MPa

Elastic modulus

23.0 °C

330 GPa

Show Supplier Material materials with Elastic modulus of 330 GPa

Hardness, Vickers

23.0 °C

2040 [-]

Show Supplier Material materials with Hardness, Vickers of 2040 [-]

Thermal

PropertyTemperatureValue

Thermal conductivity

23.0 °C

45 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 45 W/(m·K)

Technological properties

Property
Application areas

It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components.

Processing methods

pressureless sintering, reaction-bonded sintering, recrystallization sintering