Titanium Aluminium Vanadium Ti90Al6V4 Powder (TI016010/4)

.XLSX
.PDF
Save

Description

Titanium/Aluminium/Vanadium powder of spherical particle size produced by Plasma Atomization Process.

Chemical properties

Element

Weight %

Comment

Ti

-

balance

Al

6.18 %

V

4.34 %

Other

0.4 %

O

0.09 %

More

Technological properties

Other

The key benefits are: Highly spherical/flowable, few satellites/voids, excellent packing density. Sieve analysis: -60/+100 mesh (150-250µm) 94.2%

Processing history

Plasma Atomization Process

This material data has been provided by Goodfellow.