General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.9 g/cm³ Show Supplier Material materials with Density of 3.9 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Compressive strength | 23.0 °C | 2500 MPa Show Supplier Material materials with Compressive strength of 2500 MPa |
Elastic modulus | 23.0 °C | 360 GPa Show Supplier Material materials with Elastic modulus of 360 GPa |
Flexural strength | 23.0 °C | 350 MPa Show Supplier Material materials with Flexural strength of 350 MPa |
Hardness, Vickers | 23.0 °C | 1764 [-] Show Supplier Material materials with Hardness, Vickers of 1764 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 - 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 - 5 MPa·√m |
Poisson's ratio | 23.0 °C | 0.23 [-] Show Supplier Material materials with Poisson's ratio of 0.23 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.2E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.2E-6 1/K |
Specific heat capacity | 23.0 °C | 800 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 800 J/(kg·K) |
Thermal conductivity | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Thermal conductivity of 30 W/(m·K) |
Thermal shock parameter R2 | 220 W/m Show Supplier Material materials with Thermal shock parameter R2 of 220 W/m |
Electrical
Property | Temperature | Value |
---|---|---|
Dielectric constant | 23.0 °C | 9.8 [-] Show Supplier Material materials with Dielectric constant of 9.8 [-] |
Dielectric strength | 23.0 °C | 17 kV/mm Show Supplier Material materials with Dielectric strength of 17 kV/mm |
Electrical resistivity | 23.0 °C | 1.00E+20 Ω·m Show Supplier Material materials with Electrical resistivity of 1.00E+20 Ω·m |
Loss tangent | 23.0 °C | 1E-4 [-] Show Supplier Material materials with Loss tangent of 1E-4 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Wear ceramic parts: Ceramic Nozzles, Ceramic, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies | |
Processing methods | Cold Isostatic Press, Dry Press, Tape Casting, Precision Machining Processing |