General
Property | Temperature | Value |
---|---|---|
Bulk density | 23.0 °C | 0.03 - 0.04 g/cm³ Show Material materials with Bulk density of 0.03 - 0.04 g/cm³ |
Flake thickness | 0.3 - 1.7 nm Show Material materials with Flake thickness of 0.3 - 1.7 nm | |
Lateral flake size | 400 - 550 nm Show Material materials with Lateral flake size of 400 - 550 nm | |
Layer number | 1 - 5 [-] Show Material materials with Layer number of 1 - 5 [-] | |
Pore volume | 0.16 cm³/g Show Material materials with Pore volume of 0.16 cm³/g | |
Specific surface area | 300 - 340 m²/g Show Material materials with Specific surface area of 300 - 340 m²/g |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 5965 - 6215 S/m Show Material materials with Electrical conductivity of 5965 - 6215 S/m |
Chemical properties
Property | Value |
---|---|
Carbon | 97.6 - 98 % Show Material materials with Carbon of 97.6 - 98 % |
Hydrogen | 0.66 - 0.7 % Show Material materials with Hydrogen of 0.66 - 0.7 % |
Nitrogen | 0.26 - 0.32 % Show Material materials with Nitrogen of 0.26 - 0.32 % |
Oxygen | 0.98 - 1 % Show Material materials with Oxygen of 0.98 - 1 % |
Technological properties
Property | ||
---|---|---|
Processing history | No catalyst impurities |