Free Standing aligned CNT arrays (Carpets) are synthesized by floating catalyst CVD method within a horizontal quartz reaction tube.


The CNT synthesis parameters are carefully selected to provide maximum-yield of CNT growth, high packing density as well as high graphitization level.

Properties

General

Graphitization level Id/Ig

0.3 - 0.4 [-]

Dimension

Nanotube diameter dnano

30 - 90 nm

Nanotube length lnano

300 - 1000 µm

Thermal

Oxidation threshold Toxi

600 - 700 °C