Dimension
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanical
Property | Value | Comment |
---|---|---|
Tensile strength | 180 - 220 MPa Show Supplier Material materials with Tensile strength of 180 - 220 MPa | |
Yield strength | 160 MPa Show Supplier Material materials with Yield strength of 160 MPa | RP02 |
Thermal
Property | Value |
---|
Electrical
Property | Value | Comment |
---|---|---|
Corrosion potential | -880 mV Show Supplier Material materials with Corrosion potential of -880 mV | |
Electrical resistivity | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with Electrical resistivity of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Copper | 0 - 0.05 % Show Supplier Material materials with Copper of 0 - 0.05 % |
Iron | 0 - 0.4 % Show Supplier Material materials with Iron of 0 - 0.4 % |
Magnesium | 0 - 0.05 % Show Supplier Material materials with Magnesium of 0 - 0.05 % |
Manganese | 1.4 - 1.8 % Show Supplier Material materials with Manganese of 1.4 - 1.8 % |
Silicon | 0.65 - 1 % Show Supplier Material materials with Silicon of 0.65 - 1 % |
Zinc | 0.5 - 0.9 % Show Supplier Material materials with Zinc of 0.5 - 0.9 % |
Zirconium | 0.05 - 0.2 % Show Supplier Material materials with Zirconium of 0.05 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: H14SR |