TPU 3065D

Alternative and trade names
3065D
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 3065D is a polyether based thermoplastic polyurethane. ISOTHANE 3065D exhibits excellent mechanical properties, hydrolytic resistance, fungus resistance, and low temperature performance properties. ISOTHANE 3065D can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.17 g/cm³

Show Supplier Material materials with Density of 1.17 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

400.0 %

Show Supplier Material materials with Elongation of 400.0 %

ASTM D412

Hardness, Shore D

65.0 [-]

Show Supplier Material materials with Hardness, Shore D of 65.0 [-]

ASTM D2240

Tear strength

240.0 kN/m

Show Supplier Material materials with Tear strength of 240.0 kN/m

ASTM D624

Tensile strength

52.0 MPa

Show Supplier Material materials with Tensile strength of 52.0 MPa

ASTM D412

Technological properties

Property
Application areas

Apparel Applications And Outdoor Applications.