TPU 3085A-FRT

Alternative and trade names
TPU FR
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 3085A-FRT have good initial adhesive strength, fast crystallization, good solubility, good washing durability and freezing resistance. Viscosity ranges from 150~2800cps (15% MEK Solution), and viscosity could be customized for different viscosity. ISOTHANE 3085A-FRT exhibits good adhesive with TPU, PVC, polyester fabric, leather and other materials.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

700.0 %

Show Supplier Material materials with Elongation of 700.0 %

ASTM D412

Hardness, Shore A

84.0 [-]

Show Supplier Material materials with Hardness, Shore A of 84.0 [-]

ASTM D2240

Tear strength

120.0 kN/m

Show Supplier Material materials with Tear strength of 120.0 kN/m

ASTM D624

Tensile strength

33.0 MPa

Show Supplier Material materials with Tensile strength of 33.0 MPa

ASTM D412

Thermal

PropertyValue

Flammability

UL94 V0 (2mm)

Technological properties

Property
Application areas

Building/Construction, Mining, Wire and Cables