PP PL6350

Alternative and trade names
PL6350
Want to keep this datasheet? Save it now in your required format

Description

PL6350 is a glass fiber reinforced polyamide and has excellent rigidity stiffness and impact resistance. It can be used to replace the metal material of the industrial parts and efficiently lightening the weight. The surface of the product will have nice gloss and smooth. The abrasion resistance and size’s stability are better than other compoundings.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.33 g/cm³

Show Supplier Material materials with Density of 1.33 g/cm³

Mechanical

PropertyTemperatureValue

Flexural modulus

9.84 GPa

Show Supplier Material materials with Flexural modulus of 9.84 GPa

Flexural strength

192.0 MPa

Show Supplier Material materials with Flexural strength of 192.0 MPa

Impact strength, Izod notched, ASTM

-20 °C

246 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 246 J/m

23 °C

256 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 256 J/m

Tensile strength

108.0 MPa

Show Supplier Material materials with Tensile strength of 108.0 MPa

Thermal

PropertyValuePressureComment

Heat deflection temperature

155.0 °C

Show Supplier Material materials with Heat deflection temperature of 155.0 °C

1.8 MPa

ASTM D648

Rheological Properties

PropertyValue

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

Technological properties

Property
Application areas

Car Industry, Frame in the engine bay, Seat frame, Dashboard frame, Frame of Battery base, Door panel, Pedals, Fender apron, Frame of spare tire. Electronics, High precision plug-in/element, Structure parts of the printer, Frame of the 3C products, Structure parts. Petrochemical, Corrosion and abrasion resistance parts, Grille platform, Parts of filtration facility, Reactor parts. Others, Seat frame of bicycle, Snowboard, Structure parts of the exercise gear and pedals, Toe of Safety boot, Safety helmet.

Fillers

50% Glass Fiber