General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.94 g/cm³ Show Supplier Material materials with Density of 0.94 g/cm³ at 23.0 °C | 23.0 °C | ASTM D1505 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 110 - 350 % Show Supplier Material materials with Elongation of 110 - 350 % at 23.0 °C | 23.0 °C | ASTM D638 |
Flexural modulus | 0.23 - 0.88 GPa Show Supplier Material materials with Flexural modulus of 0.23 - 0.88 GPa at 23.0 °C | 23.0 °C | ASTM D790 |
Hardness, Shore D | 58 [-] Show Supplier Material materials with Hardness, Shore D of 58 [-] at 23.0 °C | 23.0 °C | ASTM D2240 |
Impact strength, Izod notched, ASTM | 220 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 220 J/m at 23.0 °C | 23.0 °C | ASTM D256 |
Tensile strength | 11.75 MPa Show Supplier Material materials with Tensile strength of 11.75 MPa at 23.0 °C | 23.0 °C | ASTM D638 |
Yield strength | 20.5 - 21 MPa Show Supplier Material materials with Yield strength of 20.5 - 21 MPa at 23.0 °C | 23.0 °C | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Vicat softening temperature | 118 °C Show Supplier Material materials with Vicat softening temperature of 118 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 3.8 g/10min Show Supplier Material materials with Melt mass-flow rate of 3.8 g/10min | ASTM D1238, 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3938 is suggested for the production of wide variety of tank applications for the storage of water, chemicals & Oils. GREENETHENE G-3938 can also be used for off-shore flotation buoys and road crash barriers. | |
Certifications | List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996 | |
Color | Natural, black, terracotta, fire red, yellow and blue. | |
Processing methods | Compression molded & rotomolded |