General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 13.24 g/cm³ Show Supplier Material materials with Density of 13.24 g/cm³ | |
Grain size | 2 - 3 μm Show Supplier Material materials with Grain size of 2 - 3 μm | tungsten carbide grain size | |
Particle size D90 | 16 μm Show Supplier Material materials with Particle size D90 of 16 μm | max |
Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Vickers, 30 | 23.0 °C | 1145 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 1145 [-] |
Magnetic
Property | Temperature | Value |
---|---|---|
Coercive force | 23.0 °C | 10188 A/m Show Supplier Material materials with Coercive force of 10188 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.015 % Show Supplier Material materials with Aluminium of 0.015 % | max | |
Carbon | as WC balance | ||
Chromium | 0.15 % Show Supplier Material materials with Chromium of 0.15 % | max | |
Cobalt | 6.5 - 8.5 % Show Supplier Material materials with Cobalt of 6.5 - 8.5 % | ||
Copper | 5E-3 % Show Supplier Material materials with Copper of 5E-3 % | max | |
Iron | 0.15 % Show Supplier Material materials with Iron of 0.15 % | max | |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max | |
Niobium | 0.4 % Show Supplier Material materials with Niobium of 0.4 % | max | |
Oxygen | 0.25 % Show Supplier Material materials with Oxygen of 0.25 % | max | |
Tantalum | 1.3 % Show Supplier Material materials with Tantalum of 1.3 % | max | |
Titanium | 0.5 % Show Supplier Material materials with Titanium of 0.5 % | max | |
Tungsten | as WC balance | ||
Vanadium | 0.03 % Show Supplier Material materials with Vanadium of 0.03 % | max | |
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade I was developed for use in a wide range of tooling products, indexable inserts, woodworking tools or wear parts. | |
Other | Grade I has a tighter specification in cubic carbides and cobalt content compared to grade TS, as well as a significantly lower specification for its aluminium content. The small amount of 1-2 μm sized cubic carbides increases the hardness and decreases the density of the material. Thanks to the fine particle size of the powder, milling characteristics are excellent and comparable to virgin WC-Co powders. |