General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 14.46 g/cm³ Show Supplier Material materials with Density of 14.46 g/cm³ | |
Grain size | 0.5 - 0.8 μm Show Supplier Material materials with Grain size of 0.5 - 0.8 μm | tungsten carbide grain size | |
Particle size D90 | 13 μm Show Supplier Material materials with Particle size D90 of 13 μm | max |
Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Vickers, 30 | 23.0 °C | 1630 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 1630 [-] |
Magnetic
Property | Temperature | Value |
---|---|---|
Coercive force | 23.0 °C | 21492 A/m Show Supplier Material materials with Coercive force of 21492 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % | max | |
Carbon | as WC balance | ||
Chromium | 0.65 % Show Supplier Material materials with Chromium of 0.65 % | max | |
Cobalt | 5 - 8 % Show Supplier Material materials with Cobalt of 5 - 8 % | ||
Copper | 5E-3 % Show Supplier Material materials with Copper of 5E-3 % | max | |
Iron | 0.15 % Show Supplier Material materials with Iron of 0.15 % | max | |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max | |
Niobium | 0.1 % Show Supplier Material materials with Niobium of 0.1 % | max | |
Oxygen | 0.35 % Show Supplier Material materials with Oxygen of 0.35 % | max | |
Tantalum | 0.1 % Show Supplier Material materials with Tantalum of 0.1 % | max | |
Titanium | 0.1 % Show Supplier Material materials with Titanium of 0.1 % | max | |
Tungsten | as WC balance | ||
Vanadium | 0.3 % Show Supplier Material materials with Vanadium of 0.3 % | max | |
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade S was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Grade S powder has an uniform WC grain size distribution with evenly distributed WC and Cobalt particles. Due to the fine particle size of the powder, milling characteristics are excellent and comparable to virgin WC-Co powders. |