General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10.8 g/cm³ Show Supplier Material materials with Density of 10.8 g/cm³ |
Dimension
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 106 GPa Show Supplier Material materials with Elastic modulus of 106 GPa | |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | max. |
Hardness, Vickers | 23.0 °C | 320 - 390 [-] Show Supplier Material materials with Hardness, Vickers of 320 - 390 [-] | |
Tensile strength | 23.0 °C | 1000 - 1350 MPa Show Supplier Material materials with Tensile strength of 1000 - 1350 MPa |
Thermal
Property | Value |
---|---|
Melting point | 1070 - 1130 °C Show Supplier Material materials with Melting point of 1070 - 1130 °C |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 2.45E-7 - 2.62E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 2.45E-7 - 2.62E-7 Ω·m |
Specific Electrical conductivity | 6.6 - 7 % IACS Show Supplier Material materials with Specific Electrical conductivity of 6.6 - 7 % IACS | |
Temperature coefficient of resistance | 23.0 °C | 3.9E-4 1/K Show Supplier Material materials with Temperature coefficient of resistance of 3.9E-4 1/K |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Potentiometers, battery contacts | |
Corrosion properties | Corrosion resistant | |
Other | Superb sliding contact alloy, stable contact resistance, wear resistant, Oxidation resistant up to 300 °C, Ductile, Age hardenable |