General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 11.8 g/cm³ Show Supplier Material materials with Density of 11.8 g/cm³ |
Dimension
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 108 GPa Show Supplier Material materials with Elastic modulus of 108 GPa | |
Elongation | 23.0 °C | 15 % Show Supplier Material materials with Elongation of 15 % | min. |
Hardness, Vickers | 23.0 °C | 190 - 240 [-] Show Supplier Material materials with Hardness, Vickers of 190 - 240 [-] | |
Shear modulus | 23.0 °C | 40 GPa Show Supplier Material materials with Shear modulus of 40 GPa | |
Tensile strength | 23.0 °C | 700 - 850 MPa Show Supplier Material materials with Tensile strength of 700 - 850 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.46E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.46E-5 1/K | RT-100 °C |
Melting point | 1130 - 1180 °C Show Supplier Material materials with Melting point of 1130 - 1180 °C | ||
Thermal conductivity | 23.0 °C | 28 W/(m·K) Show Supplier Material materials with Thermal conductivity of 28 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 3.38E-7 - 3.59E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 3.38E-7 - 3.59E-7 Ω·m |
Specific Electrical conductivity | 4.8 - 5.1 % IACS Show Supplier Material materials with Specific Electrical conductivity of 4.8 - 5.1 % IACS | |
Temperature coefficient of resistance | 23.0 °C | 2.8E-4 1/K Show Supplier Material materials with Temperature coefficient of resistance of 2.8E-4 1/K |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Potentiometers, probe pins | |
Corrosion properties | Corrosion resistant | |
Other | Superb sliding contact alloy, stable contact resistance, wear resistant, Oxidation resistant up to 300 °C, Ductile |