General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 15.1 g/cm³ Show Supplier Material materials with Density of 15.1 g/cm³ |
Dimension
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 87 GPa Show Supplier Material materials with Elastic modulus of 87 GPa |
Elongation | 23.0 °C | 3 - 15 % Show Supplier Material materials with Elongation of 3 - 15 % |
Hardness, Vickers | 23.0 °C | 220 - 300 [-] Show Supplier Material materials with Hardness, Vickers of 220 - 300 [-] |
Shear modulus | 23.0 °C | 37 GPa Show Supplier Material materials with Shear modulus of 37 GPa |
Tensile strength | 23.0 °C | 650 - 900 MPa Show Supplier Material materials with Tensile strength of 650 - 900 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.67E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.67E-5 1/K | RT-100 °C |
Melting point | 865 - 895 °C Show Supplier Material materials with Melting point of 865 - 895 °C | ||
Thermal conductivity | 23.0 °C | 66 W/(m·K) Show Supplier Material materials with Thermal conductivity of 66 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 1.25E-7 - 1.45E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 1.25E-7 - 1.45E-7 Ω·m |
Specific Electrical conductivity | 11.9 - 13.8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 11.9 - 13.8 % IACS | |
Temperature coefficient of resistance | 23.0 °C | 5.2E-4 1/K Show Supplier Material materials with Temperature coefficient of resistance of 5.2E-4 1/K |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes, Resistance wires | |
Corrosion properties | Corrosion resistant | |
Other | Wear resistant, Age hardenable, Ductile, High electrical conductivity, Stable Contact resistant |