Density
ρ20 g/cm³ at 23 °C
Creep strength
Rm,creep10,000 h (extrapolated data)
Melting point
Tm1840 - 1870 °C
Thermal conductivity
λ40.1 W/(m·K) at 20 °C
Electrical resistivity
ρel2.1E-7 Ω·m at 20 °C
This material data has been provided by Heraeus.