General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 19.87 g/cm³ Show Supplier Material materials with Density of 19.87 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Creep strength | 1200.0 °C | 7.6 MPa Show Supplier Material materials with Creep strength of 7.6 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 6.8 MPa Show Supplier Material materials with Creep strength of 6.8 MPa | 10,000 h (extrapolated data) | |
1600.0 °C | 4.6 MPa Show Supplier Material materials with Creep strength of 4.6 MPa | 10,000 h (extrapolated data) | |
Elastic modulus | 1200.0 °C | 142.2 GPa Show Supplier Material materials with Elastic modulus of 142.2 GPa | |
Elongation | 1200.0 °C | 28 % Show Supplier Material materials with Elongation of 28 % | |
1400.0 °C | 32 % Show Supplier Material materials with Elongation of 32 % | ||
1600.0 °C | 56 % Show Supplier Material materials with Elongation of 56 % | ||
Hardness, Vickers | 23.0 °C | 130 [-] Show Supplier Material materials with Hardness, Vickers of 130 [-] | |
Norton Exponent | 1200.0 °C | 6.7 [-] Show Supplier Material materials with Norton Exponent of 6.7 [-] | |
1400.0 °C | 11.6 [-] Show Supplier Material materials with Norton Exponent of 11.6 [-] | ||
1600.0 °C | 11 [-] Show Supplier Material materials with Norton Exponent of 11 [-] | ||
Tensile strength | 1200.0 °C | 85 MPa Show Supplier Material materials with Tensile strength of 85 MPa | |
1400.0 °C | 52 MPa Show Supplier Material materials with Tensile strength of 52 MPa | ||
1600.0 °C | 31 MPa Show Supplier Material materials with Tensile strength of 31 MPa | ||
Yield strength Rp0.2 | 1200.0 °C | 57 MPa Show Supplier Material materials with Yield strength Rp0.2 of 57 MPa | |
1400.0 °C | 40 MPa Show Supplier Material materials with Yield strength Rp0.2 of 40 MPa | ||
1600.0 °C | 27 MPa Show Supplier Material materials with Yield strength Rp0.2 of 27 MPa | ||
Thermal
Property | Temperature | Value |
---|---|---|
Melting point | 1840 - 1870 °C Show Supplier Material materials with Melting point of 1840 - 1870 °C | |
Thermal conductivity | 20.0 °C | 40.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of 40.3 W/(m·K) |
1200.0 °C | 66.7 W/(m·K) Show Supplier Material materials with Thermal conductivity of 66.7 W/(m·K) | |
1400.0 °C | 69.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 69.5 W/(m·K) | |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 1.5E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 1.5E-7 Ω·m |
1156.0 °C | 5.5E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 5.5E-7 Ω·m | |
1400.0 °C | 6.1E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 6.1E-7 Ω·m | |