Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Barium | 2E-6 % Show Supplier Material materials with Barium of 2E-6 % |
Boron | 1.5E-5 % Show Supplier Material materials with Boron of 1.5E-5 % |
Calcium | 7E-6 % Show Supplier Material materials with Calcium of 7E-6 % |
Chromium | 5E-6 % Show Supplier Material materials with Chromium of 5E-6 % |
Gallium | 2E-6 % Show Supplier Material materials with Gallium of 2E-6 % |
Iron | 5E-5 % Show Supplier Material materials with Iron of 5E-5 % |
Lead | 5E-6 % Show Supplier Material materials with Lead of 5E-6 % |
Magnesium | 5E-5 % Show Supplier Material materials with Magnesium of 5E-5 % |
Manganese | 5E-6 % Show Supplier Material materials with Manganese of 5E-6 % |
Nickel | 5E-6 % Show Supplier Material materials with Nickel of 5E-6 % |
Phosphorus | 5E-5 % Show Supplier Material materials with Phosphorus of 5E-5 % |
Silicon | 5E-5 % Show Supplier Material materials with Silicon of 5E-5 % |
Silver | 5E-6 % Show Supplier Material materials with Silver of 5E-6 % |
Titanium | 1E-5 % Show Supplier Material materials with Titanium of 1E-5 % |
Vanadium | 1E-5 % Show Supplier Material materials with Vanadium of 1E-5 % |
Zirconium | 5E-6 % Show Supplier Material materials with Zirconium of 5E-6 % |