Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Antimony | 8E-6 % Show Supplier Material materials with Antimony of 8E-6 % |
Arsenic | 5E-6 % Show Supplier Material materials with Arsenic of 5E-6 % |
Barium | 2E-6 % Show Supplier Material materials with Barium of 2E-6 % |
Beryllium | 1E-6 % Show Supplier Material materials with Beryllium of 1E-6 % |
Bismuth | 5E-6 % Show Supplier Material materials with Bismuth of 5E-6 % |
Boron | 2E-6 % Show Supplier Material materials with Boron of 2E-6 % |
Caesium | 5E-6 % Show Supplier Material materials with Caesium of 5E-6 % |
Calcium | 4E-6 % Show Supplier Material materials with Calcium of 4E-6 % |
Cerium | 1E-5 % Show Supplier Material materials with Cerium of 1E-5 % |
Chlorine | 1E-5 % Show Supplier Material materials with Chlorine of 1E-5 % |
Chromium | 4E-6 % Show Supplier Material materials with Chromium of 4E-6 % |
Cobalt | 1E-6 % Show Supplier Material materials with Cobalt of 1E-6 % |
Copper | 1E-5 % Show Supplier Material materials with Copper of 1E-5 % |
Fluorine | 1E-5 % Show Supplier Material materials with Fluorine of 1E-5 % |
Gallium | 1E-6 % Show Supplier Material materials with Gallium of 1E-6 % |
Germanium | 1E-5 % Show Supplier Material materials with Germanium of 1E-5 % |
Indium | 5E-6 % Show Supplier Material materials with Indium of 5E-6 % |
Iron | 1E-5 % Show Supplier Material materials with Iron of 1E-5 % |
Lanthanum | 6E-6 % Show Supplier Material materials with Lanthanum of 6E-6 % |
Lead | 5E-6 % Show Supplier Material materials with Lead of 5E-6 % |
Lithium | 1E-6 % Show Supplier Material materials with Lithium of 1E-6 % |
Magnesium | 1.5E-5 % Show Supplier Material materials with Magnesium of 1.5E-5 % |
Manganese | 2E-6 % Show Supplier Material materials with Manganese of 2E-6 % |
Molybdenum | 2E-6 % Show Supplier Material materials with Molybdenum of 2E-6 % |
Nickel | 5E-6 % Show Supplier Material materials with Nickel of 5E-6 % |
Phosphorus | 3E-5 % Show Supplier Material materials with Phosphorus of 3E-5 % |
Platinum | 1E-5 % Show Supplier Material materials with Platinum of 1E-5 % |
Silicon | 1E-5 % Show Supplier Material materials with Silicon of 1E-5 % |
Silver | 5E-6 % Show Supplier Material materials with Silver of 5E-6 % |
Sodium | 5E-6 % Show Supplier Material materials with Sodium of 5E-6 % |
Sulfur | 1E-5 % Show Supplier Material materials with Sulfur of 1E-5 % |
Thorium | 1E-6 % Show Supplier Material materials with Thorium of 1E-6 % |
Tin | 5E-6 % Show Supplier Material materials with Tin of 5E-6 % |
Titanium | 5E-6 % Show Supplier Material materials with Titanium of 5E-6 % |
Tungsten | 5E-6 % Show Supplier Material materials with Tungsten of 5E-6 % |
Uranium | 1E-6 % Show Supplier Material materials with Uranium of 1E-6 % |
Vanadium | 1E-5 % Show Supplier Material materials with Vanadium of 1E-5 % |
Zinc | 5E-6 % Show Supplier Material materials with Zinc of 5E-6 % |
Zirconium | 3E-6 % Show Supplier Material materials with Zirconium of 3E-6 % |