Description

Silicon Nitride (Si₃N₄) is 60% lighter than steel but strong enough to survive some of the most demanding applications in a variety of industries. This lightweight, high-strength ceramic material is used as an alternative to stainless steel, super alloys, tungsten carbides and first-generation ceramics such as Al₂O₃ and ZrO₂. It offers excellent thermal shock resistance and high fracture toughness, compatibility with nonferrous metal melts, and improved structural reliability compared to other ceramic materials.

This material data has been provided by Innovacera.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.21 g/cm³

Show Supplier Material materials with Density of 3.21 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

330 GPa

Show Supplier Material materials with Elastic modulus of 330 GPa

Flexural strength

23.0 °C

610 MPa

Show Supplier Material materials with Flexural strength of 610 MPa

Hardness, Vickers

23.0 °C

1417 [-]

Show Supplier Material materials with Hardness, Vickers of 1417 [-]

Plane-Strain Fracture Toughnes

23.0 °C

6 - 7 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 - 7 MPa·√m

Poisson's ratio

23.0 °C

0.25 [-]

Show Supplier Material materials with Poisson's ratio of 0.25 [-]

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

3E-6 - 3.2E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3E-6 - 3.2E-6 1/K

Specific heat capacity

23.0 °C

660 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 660 J/(kg·K)

Thermal conductivity

23.0 °C

15 - 20 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 15 - 20 W/(m·K)

Thermal shock parameter R2

550 W/m

Show Supplier Material materials with Thermal shock parameter R2 of 550 W/m

Electrical

PropertyTemperatureValue

Dielectric strength

23.0 °C

13 kV/mm

Show Supplier Material materials with Dielectric strength of 13 kV/mm

Electrical resistivity

23.0 °C

1.00E+16 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+16 Ω·m

Technological properties

Property
Application areas

High precision silicon nitride ceramic balls, roller for bearing, pump valve, Thermocouple Protection Sheaths, Electric heating element, Weld Location Pins

Processing methods

Gas Press Sintering, Cold Isostatic Press, Dry Press, Precision Machining Processing