General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.02 g/cm³ Show Supplier Material materials with Density of 3.02 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Compressive strength | 23.0 °C | 250 MPa Show Supplier Material materials with Compressive strength of 250 MPa |
Elastic modulus | 23.0 °C | 330 GPa Show Supplier Material materials with Elastic modulus of 330 GPa |
Hardness, Vickers | 23.0 °C | 2040 [-] Show Supplier Material materials with Hardness, Vickers of 2040 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Thermal conductivity | 23.0 °C | 45 W/(m·K) Show Supplier Material materials with Thermal conductivity of 45 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components. | |
Processing methods | pressureless sintering, reaction-bonded sintering, recrystallization sintering |