General
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Density | 1.39 g/cm³ Show Supplier Material materials with Density of 1.39 g/cm³ | ISO 1183 |
Water absorption | 0.25 % Show Supplier Material materials with Water absorption of 0.25 % | ISO 62 |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 4 GPa Show Supplier Material materials with Elastic modulus of 4 GPa | ISO 527 |
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % | ISO 527 |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | ISO 527 |
Hardness, Ball Indentation | 170 MPa Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa | ISO 2039-1 |
Hardness, Rockwell R | 96 [-] Show Supplier Material materials with Hardness, Rockwell R of 96 [-] | ISO 2039-1 |
Hardness, Shore D | 84 [-] Show Supplier Material materials with Hardness, Shore D of 84 [-] | DIN 53505 |
Impact strength, Charpy notched | 2 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m² | ISO 179 |
Impact strength, Charpy unnotched | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | min., ISO 179 |
Yield strength | 90 MPa Show Supplier Material materials with Yield strength of 90 MPa | ISO 527 |
Thermal
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 8e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-05 1/K | DIN 53752 | |||
Heat deflection temperature | 80 °C Show Supplier Material materials with Heat deflection temperature of 80 °C | 2 MPa | |||
Max service temperature | 100 °C Show Supplier Material materials with Max service temperature of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Min service temperature | -20 °C Show Supplier Material materials with Min service temperature of -20 °C | Longterm | |||
Thermal conductivity | 0.29 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.29 W/(m·K) | DIN 52612 | |||
Flammability | HB UL 94 |
Electrical
Property | Value | Comment |
---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | IEC 60112 |
Dielectric constant | 3.2 [-] Show Supplier Material materials with Dielectric constant of 3.2 [-] | DIN 53483 |
Dielectric strength | 22 kV/mm Show Supplier Material materials with Dielectric strength of 22 kV/mm | VDE 0303 |
Loss tangent | 0.014 [-] Show Supplier Material materials with Loss tangent of 0.014 [-] | DIN 53483 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts and rollers | |
Certifications | RoHS,REACH |