PEEK ISO-TECH

Alternative and trade names
ISO-PEEK
Want to keep this datasheet? Save it now in your required format

Description

ISO-PEEK is a semi-crystalline, high-performance thermoplastic, which has, next to very good mechanical properties, a high sliding performance. In addition, the material has a high temperature resistance. ISO-PEEK is often used for sliding guides and seals. The key features are:


  • High chemical resistance
  • Excellent sliding functionality
  • Very high temperature resistance
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Coefficient of friction

    0.2 [-]

    Show Supplier Material materials with Coefficient of friction of 0.2 [-]

    DIN 53375, B, Against dry running steel

    Density

    1.32 g/cm³

    Show Supplier Material materials with Density of 1.32 g/cm³

    ISO 1183

    Water absorption

    0.1 %

    Show Supplier Material materials with Water absorption of 0.1 %

    ISO 62

    Mechanical

    PropertyValueComment

    Elastic modulus

    3 GPa

    Show Supplier Material materials with Elastic modulus of 3 GPa

    ISO 527

    Elongation

    25 %

    Show Supplier Material materials with Elongation of 25 %

    ISO 527

    Flexural strength

    170 MPa

    Show Supplier Material materials with Flexural strength of 170 MPa

    ISO 178

    Hardness, Rockwell R

    99 [-]

    Show Supplier Material materials with Hardness, Rockwell R of 99 [-]

    ISO 2039-1

    Hardness, Shore D

    90 [-]

    Show Supplier Material materials with Hardness, Shore D of 90 [-]

    DIN 53505

    Impact strength, Charpy notched

    5 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

    ISO 179

    Yield strength

    95 MPa

    Show Supplier Material materials with Yield strength of 95 MPa

    ISO 527

    Impact strength, Charpy unnotched

    No break, ISO 179

    Thermal

    PropertyValuePressureComment

    Coefficient of thermal expansion

    5e-05 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 5e-05 1/K

    DIN 53752

    Heat deflection temperature

    140 °C

    Show Supplier Material materials with Heat deflection temperature of 140 °C

    2 MPa

    182 °C

    Show Supplier Material materials with Heat deflection temperature of 182 °C

    0.45 MPa

    Max service temperature

    260 °C

    Show Supplier Material materials with Max service temperature of 260 °C

    Longterm

    Long

    Short

    Min service temperature

    -40 °C

    Show Supplier Material materials with Min service temperature of -40 °C

    Longterm

    Thermal conductivity

    0.25 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.25 W/(m·K)

    DIN 52612

    Vicat softening temperature

    250 °C

    Show Supplier Material materials with Vicat softening temperature of 250 °C

    ISO 306, VST B50

    Flammability

    V-0 UL 94

    Electrical

    PropertyValueComment

    Comparative tracking index

    150 V

    Show Supplier Material materials with Comparative tracking index of 150 V

    IEC 60112

    Dielectric constant

    3.2 [-]

    Show Supplier Material materials with Dielectric constant of 3.2 [-]

    DIN 53483

    Dielectric strength

    20 kV/mm

    Show Supplier Material materials with Dielectric strength of 20 kV/mm

    VDE 0303

    Loss tangent

    0.003 [-]

    Show Supplier Material materials with Loss tangent of 0.003 [-]

    DIN 53483

    Surface resistivity

    1e+15 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq

    min., VDE 0303

    Volume resistivity

    1e+16 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+16 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas

    Sliding parts, blindings and for applications at very high temperatures

    Certifications

    Food Contact: FDA and EU 10/2011, RoHS,REACH

    UV resistance

    Partly