General
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.12 [-] Show Supplier Material materials with Coefficient of friction of 0.12 [-] | DIN 53375, A, Against dry running steel |
Density | 0.93 g/cm³ Show Supplier Material materials with Density of 0.93 g/cm³ | ISO 1183 |
Water absorption | 0.01 % Show Supplier Material materials with Water absorption of 0.01 % | ISO 62 |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 0.7 GPa Show Supplier Material materials with Elastic modulus of 0.7 GPa | min., ISO 527 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | min., ISO 527 | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | min., ISO 527 | |
Flexural strength | 27 MPa Show Supplier Material materials with Flexural strength of 27 MPa | ISO 178 | |
Hardness, Ball Indentation | 38 MPa Show Supplier Material materials with Hardness, Ball Indentation of 38 MPa | ISO 2039-1 | |
Hardness, Shore D | 63 [-] Show Supplier Material materials with Hardness, Shore D of 63 [-] | DIN 53505 | |
Tear strength | 40 kN/m Show Supplier Material materials with Tear strength of 40 kN/m | min., ISO 527 | |
Yield strength | 17 MPa Show Supplier Material materials with Yield strength of 17 MPa | ISO 527 | |
Impact strength, Charpy notched | No break, ISO 179 | ||
Impact strength, Charpy unnotched | No break, ISO 179 |
Thermal
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 0.0002 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.0002 1/K | DIN 53752 | |||
Heat deflection temperature | 42 °C Show Supplier Material materials with Heat deflection temperature of 42 °C | 2 MPa | |||
65 °C Show Supplier Material materials with Heat deflection temperature of 65 °C | 0.45 MPa | ||||
Max service temperature | 90 °C Show Supplier Material materials with Max service temperature of 90 °C | Longterm | |||
Long | |||||
Short | |||||
Min service temperature | -150 °C Show Supplier Material materials with Min service temperature of -150 °C | Longterm | |||
Thermal conductivity | 0.41 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.41 W/(m·K) | DIN 52612 | |||
Vicat softening temperature | 79 °C Show Supplier Material materials with Vicat softening temperature of 79 °C | ISO 306, VST B50 | |||
Flammability | HB UL 94 |
Electrical
Property | Value | Comment |
---|---|---|
Dielectric constant | 3 [-] Show Supplier Material materials with Dielectric constant of 3 [-] | DIN 53483 |
Dielectric strength | 45 kV/mm Show Supplier Material materials with Dielectric strength of 45 kV/mm | VDE 0303 |
Loss tangent | 0.0001 [-] Show Supplier Material materials with Loss tangent of 0.0001 [-] | DIN 53483 |
Surface resistivity | 1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+11 Ω/sq | min., VDE 0303 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |