General
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.08 [-] Show Supplier Material materials with Coefficient of friction of 0.08 [-] | DIN 53375, A, Against dry running steel |
Density | 0.93 g/cm³ Show Supplier Material materials with Density of 0.93 g/cm³ | ISO 1183 |
Water absorption | 0.01 % Show Supplier Material materials with Water absorption of 0.01 % | ISO 62 |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 0.68 GPa Show Supplier Material materials with Elastic modulus of 0.68 GPa | min., ISO 527 | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | ISO 527 | |
Flexural strength | 27 MPa Show Supplier Material materials with Flexural strength of 27 MPa | ISO 178 | |
Hardness, Ball Indentation | 35 MPa Show Supplier Material materials with Hardness, Ball Indentation of 35 MPa | ||
Hardness, Shore D | 61 [-] Show Supplier Material materials with Hardness, Shore D of 61 [-] | DIN 53505 | |
Tensile strength | 28 MPa Show Supplier Material materials with Tensile strength of 28 MPa | DIN 53455 | |
Yield strength | 17 MPa Show Supplier Material materials with Yield strength of 17 MPa | ISO 527 | |
Elongation | No break, ISO 527 | ||
Impact strength, Charpy notched | No break, ISO 179 | ||
Impact strength, Charpy unnotched | No break, ISO 179 | ||
Tear strength | No break, ISO 527 |
Thermal
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 0.0002 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.0002 1/K | DIN 53752 | |||
Heat deflection temperature | 42 °C Show Supplier Material materials with Heat deflection temperature of 42 °C | 0.45 MPa | |||
Max service temperature | 80 °C Show Supplier Material materials with Max service temperature of 80 °C | Longterm | |||
Long | |||||
Short | |||||
Min service temperature | -150 °C Show Supplier Material materials with Min service temperature of -150 °C | Longterm | |||
Thermal conductivity | 0.41 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.41 W/(m·K) | DIN 52612 | |||
Vicat softening temperature | 80 °C Show Supplier Material materials with Vicat softening temperature of 80 °C | ISO 306, VST B50 | |||
Flammability | HB UL 94 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |