T20-60 is a two-part low viscosity epoxy infusion resin developed for mass CFRP production. The resin offers simple and flexible processing due to low viscosity and room temperature impregnation. T20-60 was developed specially for vacuum infusion molding, to produce laminates with low porosity and optimal mechanical performance. It shows the following features and properties:


  • Two-part resin system for vacuum infusion and RTM
  • Wide processing window > 2 hours at 25°C
  • Curing at room temperature
  • Low exotherm
  • High crack resistance
  • Optimal price/quality ratio
  • This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.27 g/cm³

    Show Material materials with Density of 1.27 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    3.2 GPa

    Show Material materials with Elastic modulus of 3.2 GPa

    ASTM D638

    Flexural strength

    23.0 °C

    155 MPa

    Show Material materials with Flexural strength of 155 MPa

    ASTM D790

    Plane-Strain Fracture Toughnes

    23.0 °C

    0.76 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 0.76 MPa·√m

    ASTM D5045

    Tensile strength

    23.0 °C

    80 MPa

    Show Material materials with Tensile strength of 80 MPa

    ASTM D638

    Strain energy release

    ASTM D5045

    Thermal

    PropertyValueComment

    Glass transition temperature

    87 °C

    Show Material materials with Glass transition temperature of 87 °C

    ASTM E2092

    Technological properties

    Property
    Application areas

    Marine: The shells of boats and sport catamarans can be made of composite;Car tuning: The composite material provides solutions for automotive parts to be light-weighted, stylish and aesthetic;Wind energy: Wind turbines is usually made of carbon fiber plastic;Design;Room temperature tooling;High-pressure cylinders

    Processing methods

    Mix the components A and B and weight proportion 100:32. Degas the resin with intensive mixing for 15-20 minutes at 20-25°С. Maintaining resin pot temperature of 20-25°С and tool temperature of 20-25°С, begin resin infusion. Cure at room temperature for 24h. Make sure the resin is gelled. Remove auxiliary materials. Increase temperature at rate 0,5-2°С/min to 80°С. Postcure at 80°С for 3-6h.