General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Density of 1.6 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 250 GPa Show Supplier Material materials with Elastic modulus of 250 GPa |
Elongation | 23.0 °C | 1.7 % Show Supplier Material materials with Elongation of 1.7 % |
Poisson's ratio | 23.0 °C | 0.25 [-] Show Supplier Material materials with Poisson's ratio of 0.25 [-] |
Shear strength | 23.0 °C | 40 MPa Show Supplier Material materials with Shear strength of 40 MPa |
Tensile strength | 23.0 °C | 4900 MPa Show Supplier Material materials with Tensile strength of 4900 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 68% Carbon Fiber | |
Processing methods | The production process is formed by laminating hot-pressed carbon fiber prepreg. |