PA6 CF20

Alternative and trade names
PA6-CF20
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 6 (PA6) reinforced with 20% carbon fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 - 3 %

Show Supplier Material materials with Elongation of 2 - 3 %

ASTM D638

Flexural modulus

23.0 °C

11.03 GPa

Show Supplier Material materials with Flexural modulus of 11.03 GPa

ASTM D790

Flexural strength

23.0 °C

260 MPa

Show Supplier Material materials with Flexural strength of 260 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

69 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 69 J/m

ASTM D256

Tensile strength

23.0 °C

171 MPa

Show Supplier Material materials with Tensile strength of 171 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

210 °C

Show Supplier Material materials with Heat deflection temperature of 210 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.1 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.1 - 0.2 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Fillers

20% Carbon Fiber