General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ASTM D792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 60 % Show Supplier Material materials with Elongation of 60 % | ASTM D638 |
Flexural modulus | 23.0 °C | 3.52 GPa Show Supplier Material materials with Flexural modulus of 3.52 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 165 MPa Show Supplier Material materials with Flexural strength of 165 MPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Tensile strength | 23.0 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ASTM D648 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric strength | 23.0 °C | 33 kV/mm Show Supplier Material materials with Dielectric strength of 33 kV/mm | ASTM D147 |
Technological properties