POM GF30

Alternative and trade names
POM-GF30
Want to keep this datasheet? Save it now in your required format

Description

Polyoxymethylene (POM), reinforced with 30% glass fiber, is both weather and UV resistant

Properties

General

Density

ρ

1.63 g/cm³ at 20 °C

ASTM D792

Mechanical

Flexural modulus

Ebend

8.27 GPa at 20 °C

ASTM D790

Flexural strength

σbend

152 MPa at 20 °C

ASTM D790

Impact strength, Charpy notched, ASTM

Ivnot,astm

53 J/m at 20 °C

ASTM D256

Thermal

Melting point

Tm

165 °C

ASTM D2117

Electrical

Dielectric strength

EDS

20 kV/mm at 20 °C

ASTM D147

Technological properties

Filler Type

Fillers

30% Glass Fiber

Modifications

Processing Tag

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.