POM GF 40

Alternative and trade names
POM GF 40
.XLSX
.PDF
Save

Description

Homopolymerize HB Virgin Grade

Properties

General

Density ρ

1.7 g/cm³ at 20 °C

ASTM D792

Mechanical

Elongation A

3 % at 20 °C

ASTM D638

Flexural modulus Ebend

10.3 GPa at 20 °C

ASTM D790

Flexural strength σbend

159 MPa at 20 °C

ASTM D790

Impact strength, Charpy notched, ASTM Ivnot,astm

75 J/m at 20 °C

ASTM D256

Tensile strength Rm

117 MPa at 20 °C

ASTM D638

Thermal

Coefficient of thermal expansion α

3.7999999999999997E-4 1/K at 20 °C

Heat deflection temperature HDT

166 °C

ASTM D648

Electrical

Dielectric strength EDS

20 kV/mm at 20 °C

ASTM D147

Technological properties

Fillers

40% Glass Fiber

Processing methods

injection Molding

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.