ABS GF30

Alternative and trade names
ABS-GF30
Want to keep this datasheet? Save it now in your required format

Description

Acrylonitrile Butadiene Styrene (ABS) reinforced with 30% glass fiber

Properties

General

Density

ρ

1.24 g/cm³ at 20 °C

ASTM D792

Mechanical

Flexural modulus

Ebend

5.63 GPa at 20 °C

ASTM D790

Hardness, Shore D

HS D

82 [-] at 20 °C

ASTM D785

Impact strength, Charpy notched, ASTM

Ivnot,astm

64 J/m at 20 °C

ASTM D256

Tensile strength

Rm

78 MPa at 20 °C

ASTM D638

Thermal

Heat deflection temperature

HDT

103 °C

ASTM D648

Vicat softening temperature

Tsoft

115 °C

ASTM D15255

Technological properties

Filler Type

Fillers

30% Glass Fiber

Processing Tag

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.