Acrylonitrile Butadiene Styrene (ABS) reinforced with 10% carbon fiber

Properties

General

Density

ρ

1.18 g/cm³ at 20 °C

ASTM D792

Mechanical

Elongation

A

1 % at 20 °C

ASTM D638

Flexural modulus

Ebend

7.58 GPa at 20 °C

ASTM D790

Flexural strength

σbend

117 MPa at 20 °C

ASTM D790

Impact strength, Charpy notched, ASTM

Ivnot,astm

53 J/m at 20 °C

ASTM D256

Tensile strength

Rm

82.7 MPa at 20 °C

ASTM D638

Thermal

Flammability

UL 94 HB (1.6mm)

Heat deflection temperature

HDT

110 °C

ASTM D648

Technological properties

Filler Type

Fillers

10% Carbon Fiber

Processing Tag

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.