POM GB25

Alternative and trade names
POM-GB25
Want to keep this datasheet? Save it now in your required format

Description

Polyoxymethylene (POM) reinforced with 20% glass beads

Properties

General

Density

ρ

1.6 g/cm³ at 20 °C

ASTM D792

Mechanical

Flexural modulus

Ebend

3.2 GPa at 20 °C

ASTM D790

Flexural strength

σbend

83 MPa at 20 °C

ASTM D790

Impact strength, Charpy notched, ASTM

Ivnot,astm

65 J/m at 20 °C

ASTM D256

Tensile strength

Rm

44 MPa at 20 °C

ASTM D638

Thermal

Flammability

UL 94 HB (1.6mm)

Heat deflection temperature

HDT

120 °C

ASTM D648

Melting point

Tm

166 °C

ASTM D2117

Electrical

Dielectric constant

εr

3.7 [-] at 20 °C

ASTM D147

Dielectric strength

EDS

19 kV/mm at 20 °C

ASTM D147

Technological properties

Filler Type

Fillers

20% Glass Bead

Processing Tag

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.