PEI GF30

Alternative and trade names
PEI-GF30
Want to keep this datasheet? Save it now in your required format

Description

30% Glass Fiber Reinforced Polyetherimide (PEI-GF30)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.52 g/cm³

Show Supplier Material materials with Density of 1.52 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

ASTM D638

Flexural strength

23.0 °C

335 MPa

Show Supplier Material materials with Flexural strength of 335 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

90 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 90 J/m

ASTM D256

Tensile strength

23.0 °C

245 MPa

Show Supplier Material materials with Tensile strength of 245 MPa

ASTM D638

Flexural modulus

ASTM D790

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ASTM D648

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.2 - 0.4 %

Show Supplier Material materials with Shrinkage of 0.2 - 0.4 %

Technological properties

Property
Application areas

Handles of surgical equipment, fixtures, prostheses, medical light reflectors, dental appliances etc

Fillers

30% Glass Fiber