Description

30% Glass Fiber Reinforced Thermoplastic Polyurethane (TPU-GF30)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.39 g/cm³

Show Supplier Material materials with Density of 1.39 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

15 %

Show Supplier Material materials with Elongation of 15 %

ASTM D638

Flexural modulus

23.0 °C

6.21 GPa

Show Supplier Material materials with Flexural modulus of 6.21 GPa

ASTM D790

Flexural strength

23.0 °C

179 MPa

Show Supplier Material materials with Flexural strength of 179 MPa

ASTM D790

Hardness, Shore D

23.0 °C

72 [-]

Show Supplier Material materials with Hardness, Shore D of 72 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

150 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 150 J/m

ASTM D256

Tensile strength

23.0 °C

65 MPa

Show Supplier Material materials with Tensile strength of 65 MPa

ASTM D638

Tear strength

12.0

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

178 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C

ASTM D648

Flammability

UL94 HB

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

16 kV/mm

Show Supplier Material materials with Dielectric strength of 16 kV/mm

ASTM D147

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Application areas

Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc

Fillers

30% Glass Fiber