PA6 GF33

Alternative and trade names
PA6-GF33
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.32 g/cm³

Show Supplier Material materials with Density of 1.32 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

4 %

Show Supplier Material materials with Elongation of 4 %

ASTM D638

Flexural modulus

23.0 °C

7.54 GPa

Show Supplier Material materials with Flexural modulus of 7.54 GPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

250 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 250 J/m

ASTM D256

Tensile strength

23.0 °C

132 MPa

Show Supplier Material materials with Tensile strength of 132 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ASTM D648

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

Technological properties

Property
Application areas

Cutting machine, electric saw, electric drill, angle grinder, polisher, electric hammer, electric pick, hot air gun, lithium battery screwdriver, sanding machine, engraving machine, etc.;   cooling water chamber, intake manifold, mirror frame bracket, pass style Barriers, door handles, throttle bodies, fan covers, shift lever covers, hand brakes, accelerator pedals, gears, etc.; water pumps, water valves, bearings, bushings, gears, brackets, rollers, etc.; ski equipment, strollers, bicycles , Seat bracket, pulley, shaft, shredder gear, printer parts, etc.

Fillers

33% Glass Fiber