PP GF20 LFT-G ®

Alternative and trade names
LFT-G ® PP-NA-LGF20, PP-LGF20 FR
Want to keep this datasheet? Save it now in your required format

Description

PP (HPP Polypropylene) with 20% long glass fiber reinforced. The key features are:


  • Excellent anti creeep and fatigue resistance
  • Low warpage
  • Chemical coupling
  • High strength

  • Heat resistant, UV resistant and flame retardant grades are available.

    This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1 g/cm³

    Show Supplier Material materials with Density of 1 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    4.3 GPa

    Show Supplier Material materials with Elastic modulus of 4.3 GPa

    ASTM D638

    Elongation

    23.0 °C

    6.7 %

    Show Supplier Material materials with Elongation of 6.7 %

    ASTM D638

    Flexural modulus

    23.0 °C

    3.97 GPa

    Show Supplier Material materials with Flexural modulus of 3.97 GPa

    ASTM D790

    Flexural strength

    23.0 °C

    139 MPa

    Show Supplier Material materials with Flexural strength of 139 MPa

    ASTM D790

    Impact strength, Izod notched

    23.0 °C

    29 kJ/m²

    Show Supplier Material materials with Impact strength, Izod notched of 29 kJ/m²

    ISO 179

    Tensile strength

    23.0 °C

    109 MPa

    Show Supplier Material materials with Tensile strength of 109 MPa

    ASTM D638

    Rheological Properties

    PropertyTemperatureValueComment

    Shrinkage

    23.0 °C

    0.3 - 0.5 %

    Show Supplier Material materials with Shrinkage of 0.3 - 0.5 %

    ASTM D955, (1/8 in (3.2 mm)section)

    Technological properties

    Property
    Application areas

    For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal, Washing machine drum, Water pump parts, Water treatment components, Furniture parts.

    Fillers

    20% Long Glass Fiber

    Processing methods

    Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C