VYPET™ VNT-615 FR

Alternative and trade names
PET-GF15
Want to keep this datasheet? Save it now in your required format

Description

Polyethylene Terephthalate (PET) with 15% Glass Fiber Reinforced and Flame Retardant, 45% PCR

This material data has been provided by Lavergne.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.55 g/cm³

Show Supplier Material materials with Density of 1.55 g/cm³

ASTM D792

Recycled Content

45 %

Show Supplier Material materials with Recycled Content of 45 %

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

5.9 GPa

Show Supplier Material materials with Flexural modulus of 5.9 GPa

ISO 178, 2 mm/min

Flexural strength

23.0 °C

150 MPa

Show Supplier Material materials with Flexural strength of 150 MPa

ISO 178, 2 mm/min

Impact strength, Izod notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180

Tensile strength

23.0 °C

105 MPa

Show Supplier Material materials with Tensile strength of 105 MPa

ISO 527, 5 mm/min

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

15 %

Show Supplier Material materials with Ash content of 15 %

ASTM D5630

Heat deflection temperature, 1.80 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C

ISO 75

Flammability

V0, V0 5VA for 3.2 mm sample UL94

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

37 kV/mm

Show Supplier Material materials with Dielectric strength of 37 kV/mm

ASTM D149, 1.6 mm, 500V/s in oil

Dissipation factor, 1kHz

23.0 °C

2E-3 [-]

Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-]

ASTM D150

Volume resistivity

23.0 °C

1.00E+18 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+18 Ω·cm

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

ASTM D955

Shrinkage, transverse

23.0 °C

0.9 %

Show Supplier Material materials with Shrinkage, transverse of 0.9 %

ASTM D955

Technological properties

Property
Application areas

Electrical components, appliances and structral applications.

Certifications

RoHS,RECH

Color

Black

Fillers

15% Glass Fiber and Mineral Powder

Processing methods

  • Drying to Dew Point:-18°C or lower
  • Feed zone: 260-270°C
  • Middle zone: 265-275°C
  • Front zone: 270-290°C
  • Nozzle: 275-295°C
  • Melt temperature: 275-295°C
  • Mold temperature (thick wall parts): 95-120°C
  • Mold temperature (thin wall parts): 95-120°C
  • Injection Pressure: 55-85 MPa
  • Injection Speed: Fast
  • Back Pressure: 25-50 psi
  • Screw Speed: 50-75 rpm