General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 0.5 - 0.65 g/cm³ Show Material materials with Density of 0.5 - 0.65 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Compressive strength | 20.0 °C | 40 - 110 MPa Show Material materials with Compressive strength of 40 - 110 MPa |
Elastic modulus | 20.0 °C | 5 - 20 GPa Show Material materials with Elastic modulus of 5 - 20 GPa |
Hardness, Brinell | 20.0 °C | 45 - 63 [-] Show Material materials with Hardness, Brinell of 45 - 63 [-] |
Tensile strength | 20.0 °C | 100 - 400 MPa Show Material materials with Tensile strength of 100 - 400 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Specific heat capacity | 20.0 °C | 1400 - 1800 J/(kg·K) Show Material materials with Specific heat capacity of 1400 - 1800 J/(kg·K) |
Thermal conductivity | 20.0 °C | 0.16 - 0.22 W/(m·K) Show Material materials with Thermal conductivity of 0.16 - 0.22 W/(m·K) |
Thermal diffusivity | 20.0 °C | 0.24 - 0.62 mm²/s Show Material materials with Thermal diffusivity of 0.24 - 0.62 mm²/s |