M5 Rigid-Rod Polymer Fiber (PIPD)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

1.7 g/cm³

Show Material materials with Density of 1.7 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

344 GPa

Show Material materials with Elastic modulus of 344 GPa

Elongation

20.0 °C

2.5 %

Show Material materials with Elongation of 2.5 %

Tensile strength

20.0 °C

7200 MPa