ENVIROPLAS® ENV11-NC720

Want to keep this datasheet? Save it now in your required format

Description

ENVIROPLAS® ENV11-NC720 belongs to the polycarbonate class of polymers and is an environmentally-friendly product by Enviroplas. It has superior impact strength, excellent heat resistance, and low-temperature toughness with good electrical and thermal properties.
ENVIROPLAS® ENV11-NC720 is a non-halogenated flame retardant (UL94 V0) grade and shows good mold release. It is UV stabilized, and thus exhibits good UV resistance. It is also known in particular for its use in lighting applications, casting a soft, evenly diffused light in LED lights.
Key features of ENV11-NC720 include:

  • Injection molding grade
  • Non-halogenated
  • Flame retardant
  • UV stabilized
  • Mold release
  • Excellent dimensional stability

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

80 %

Show Material materials with Elongation of 80 %

ASTM D638

Flexural modulus

23.0 °C

2.3 GPa

Show Material materials with Flexural modulus of 2.3 GPa

ASTM D790

Flexural strength

23.0 °C

93.07 MPa

Show Material materials with Flexural strength of 93.07 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

693 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 693 J/m

ASTM D256

Yield strength

23.0 °C

66.18 MPa

Show Material materials with Yield strength of 66.18 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

124 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 124 °C

ASTM D648, unannealed

Flammability

V-0 for 1.52 mm and 5VA for 3 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

16 g/10min

Show Material materials with Melt mass-flow rate of 16 g/10min

300°C/1.2 Kg

Shrinkage

23.0 °C

5E-3 - 7E-3 %

Show Material materials with Shrinkage of 5E-3 - 7E-3 %

ASTM D955

Technological properties

Property
Application areas

Lighting applications

Color

translucent-opaque

Processing methods

Injection Molding, Drying Temperature: 120°C, Drying Time: 3-4 hr, Rear Temperature: 250-265°C, Middle Temperature: 265-276°C, Front Temperature: 265-276°C, Nozzle Temperature: 240-265°C, Mold Temperature: 68-93°C, Back Pressure: 0.34-0.68 MPa, Screw Speed: 40-70 rpm