SABIC® PS 325

Want to keep this datasheet? Save it now in your required format

Description

PS 325 is High Impact Polystyrene manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resistance property. It is generally opaque in color. It is having medium flow characteristics with high tensile and flexural strength with medium heat deflection and vicat temperatures.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.6 g/cm³

Show Material materials with Bulk density of 0.6 g/cm³

ASTM D 1895

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.16 GPa

Show Material materials with Elastic modulus of 2.16 GPa

ASTM D638

Elongation

23.0 °C

50 %

Show Material materials with Elongation of 50 %

ASTM D638

Flexural modulus

23.0 °C

2.35 GPa

Show Material materials with Flexural modulus of 2.35 GPa

ASTM D 790

Flexural strength

23.0 °C

35 MPa

Show Material materials with Flexural strength of 35 MPa

ASTM D790

Hardness, Rockwell L

23.0 °C

60 [-]

Show Material materials with Hardness, Rockwell L of 60 [-]

ASTM D785

Tensile strength

23.0 °C

22 MPa

Show Material materials with Tensile strength of 22 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

93 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 93 °C

ASTM D648

Vicat softening temperature

95 °C

Show Material materials with Vicat softening temperature of 95 °C

ASTM D 1525 | Rate A/50°C

Technological properties

Property
Application areas

Air Conditioning,Amusement Machine,ATM/Ticket Machine,Auto Aftermarket,Circuit Protection,Cluster,Console,Cooking Range,Data Transfer,Dishwasher,Document Handling,Door Handle,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exterior Mirror,Fluid Delivery,Food Transportation,Forward Lighting,Gas/Electric Oven,Heavy Vehicles,Hygiene/Personal Care,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Meter Gas,Meter Water,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Personal Computing,Power Manangement,Rear/Signal Lighting,Refrigerator,Respiratory,Small Appliance,Surgical Devices,Swimming Pool/Spa,Trim,Watch/Jewelry,Wireless Communications,Wiring Devices,Irrigation,Wire & cable