SABIC® PP 576S

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP 576S is a PP homopolymer grade that has good flow properties, very good demoulding properties and a narrow molecular weight distribution. Products made from SABIC® PP 576S typically have low warpage and a high gloss, high stiffness in combination with moderate impact strength at room temperature. Application: SABIC® PP 576S is typically used in caps & closures and thin wall packaging both in food and non-food segments, and appliances. Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site http://www.SABIC.com The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. This grade material is UL registered under File E111275 (www.ul.com) IMDS 7172624

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

71 [-]

Show Material materials with Hardness, Shore D of 71 [-]

ISO 868

Technological properties

Property
Application areas

It is typically used in caps & closures and thin wall packaging both in food and non-food segments, and appliances.