SABIC® LLDPE 6318BJ

Want to keep this datasheet? Save it now in your required format

Description

6318BJ resin is a hexene comonomer based Linear Low Density Polyethylene TNPP free grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures used during production of Cast films. Films produced using this resin gives excellent optical properties, toughness, puncture resistance and tear strength.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Vicat softening temperature

99 °C

Show Material materials with Vicat softening temperature of 99 °C

ASTM D1525

Optical

PropertyValueComment

Haze

4 %

Show Material materials with Haze of 4 %

ASTM D1003

Technological properties

Property
Application areas

Blown film,General purpose film