SABIC® PP 651H

Want to keep this datasheet? Save it now in your required format

Description

PP 651H is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) green colored & specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance with improved throughput & gloss.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Material materials with Density of 0.9 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

13 %

Show Material materials with Elongation at yield of 13 %

ISO 527-1/-2

Flexural modulus

23.0 °C

0.9 GPa

Show Material materials with Flexural modulus of 0.9 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

93 [-]

Show Material materials with Hardness, Rockwell L of 93 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

220 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 220 J/m

ASTM D256

Yield strength

23.0 °C

28 MPa

Show Material materials with Yield strength of 28 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

80 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 80 °C

ASTM D648

Vicat softening temperature

135 °C

Show Material materials with Vicat softening temperature of 135 °C

ASTM D1525

Technological properties

Property
Application areas

Specially designed for transport of hot and cold drinking water.

Color