SABIC® HDPE B5403

Want to keep this datasheet? Save it now in your required format

Description

B5403 is a High Density Polyethylene specially developed for blow molding / Jerry cans and drums. The material offers and excellent combination of stiffness and ESCR and a high Impact resistance. This grade can be used in food contact applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.2 GPa

Show Material materials with Elastic modulus of 1.2 GPa

ASTM D638

Elongation at yield

23.0 °C

8 %

Show Material materials with Elongation at yield of 8 %

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

80 kJ/m²

Show Material materials with Impact strength, Charpy notched of 80 kJ/m²

ISO 179

Impact strength, Izod notched

-30.0 °C

290 kJ/m²

Show Material materials with Impact strength, Izod notched of 290 kJ/m²

ISO 8256

Yield strength

23.0 °C

27 MPa

Show Material materials with Yield strength of 27 MPa

ASTM D638

Technological properties

Property
Application areas

Jerry cans, drums