SABIC® FORTIFY™ C13060D

Want to keep this datasheet? Save it now in your required format

Description

SABIC® FORTIFY™ C13060D is an ethylene octene copolymer produced by solution polymerization using metallocene catalyst. This product is available as free flowing pellets. SABIC® FORTIFY™ C13060D is designed as alow density and high performance copolymer modifier to provide superior impact properties and flow characteristics.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

0.863 g/cm³

Show Material materials with Density of 0.863 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Flexural modulus

0.0075 GPa

Show Material materials with Flexural modulus of 0.0075 GPa

ASTM D790 A | (1% Secant)

Tear strength

25.5 kN/m

Show Material materials with Tear strength of 25.5 kN/m

ASTM D624

Thermal

PropertyValueComment

Glass transition temperature

-56.0 °C

Show Material materials with Glass transition temperature of -56.0 °C

SABIC method

Melting point

42.0 °C

Show Material materials with Melting point of 42.0 °C

SABIC method

Rheological Properties

PropertyValueComment

Mooney viscosity

3.0 MU

Show Material materials with Mooney viscosity of 3.0 MU

ASTM D1646 | ML 1+4, 121 °C

Technological properties

Property
Application areas

Wire & cable,Impact modification