SABIC HDPE CC254 is state of the art resin produced by ACP technology. It is easy to process on injection molding and compression molding machines. The grade offers good balance of stiffness, toughness and environmental stress cracking resistance properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.15 GPa

Show Material materials with Elastic modulus of 1.15 GPa

ASTM D638

Elongation at yield

23.0 °C

10 %

Show Material materials with Elongation at yield of 10 %

ISO 527-1/-2

Hardness, Shore D

23.0 °C

62 [-]

Show Material materials with Hardness, Shore D of 62 [-]

ASTM D2240

Impact strength, Charpy notched

-30.0 °C

5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179

Yield strength

23.0 °C

30 MPa

Show Material materials with Yield strength of 30 MPa

ASTM D638

Technological properties

Property
Application areas

Collapsible tubes,Caps & closures