SABIC® PP FPC100

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP FPC100 has been developed as a new member of the SABIC® PP FLOWPACT range dedicated to the thin wall packaging market. It is nucleated and is characterized by a high crystallization temperature and excellent flow behaviour in combination with a nice stiffness to impact balance. This grade is typically used for high-speed injection moulding and it enables very cost efficient processing on the basis of easy mould filling and very short cycle times. It has a very good antistatic performance and permitseasy demoulding.This material is typically used in thin wall packing applications both for food and non-food segments. This includes yellow fats/margarine tubs, dairy packaging and housewares. The grade has an excellent dimensional stability what is crucial for the thin wall packaging market. Health, Safety and Food Contact regulations:Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site http://www.SABIC.comThe product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. IMDS 80775790

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

62 [-]

Show Material materials with Hardness, Shore D of 62 [-]

ISO 868

Technological properties

Property
Application areas

This grade is typically used for high-speed injection moulding and it enables very cost efficient processing on the basis of easy mould filling and very short cycle times. It has a very good antistatic performance and permitseasy demoulding.This material is typically used in thin wall packing applications both for food and non-food segments. This includes yellow fats/margarine tubs, dairy packaging and housewares. The grade has an excellent dimensional stability what is crucial for the thin wall packaging market.